How-to

Fabric Shrinkage Test: Method, Formula and Report

How to run a fabric shrinkage test: marking, washing, the shrinkage % formula with worked examples, a report format and how to adjust patterns for shrinkage.

Quick answer: A fabric shrinkage test marks a sample (often 50 cm gauge lengths in warp and weft), washes and dries it to the buyer's method, such as ISO 6330 with ISO 5077 or AATCC 135, and re-measures. Shrinkage % = (after − before) ÷ before × 100; negative is shrinkage, positive is growth. The buyer sets the acceptable limit.

By Radiatus team · Published 04 Nov 2026 · Updated 04 Nov 2026 · 9 min read

A fabric shrinkage test measures how much a fabric changes in length and width after it is washed and dried the way the finished garment will be. You mark a sample, wash and dry it by a stated method, measure it again, and express the change as a percentage in the warp (length) and weft (width) directions. Buyers use the result to accept or reject fabric and garment makers use it to size their patterns. This guide covers the method, the fabric shrinkage test formula with worked examples, a report format and how to compensate patterns, for QC teams in Indian mills and garment units.

What is a fabric shrinkage test?

In standards language it is a test of dimensional stability to washing, or dimensional change in washing and drying. The idea is simple: a fabric that has been stretched during knitting, weaving, dyeing or finishing will try to return to a relaxed state when it is wetted, agitated and dried. Some of that happens in the first wash, so testing the fabric before cutting tells you what the garment will do in the customer's machine.

Three international standards are usually named together, and US buyers often name the AATCC method instead:

  • ISO 3759: how to prepare, mark and measure the specimens.
  • ISO 6330: the domestic washing and drying procedures (machine type, temperature, programme, drying method).
  • ISO 5077: how to calculate and report the dimensional change.
  • AATCC 135: the US method for dimensional changes of fabrics after home laundering.

The buyer's manual says which method, wash programme, temperature, drying method and number of cycles apply. Everything below follows that pattern; the details come from the manual.

What do you need for a shrinkage test?

  • A sample cut from the full width, away from the selvedge and the roll ends, conditioned before marking.
  • A marking template (a square or a set of gauge marks) and an indelible fine marker or stitched marks that will survive washing.
  • A ruler or tape that reads to 1 mm.
  • A washing machine and programme as the method specifies (for example an ISO 6330 reference machine and programme, or a domestic machine where the buyer allows an in-house check).
  • A drying method: line dry, flat dry or tumble dry, as specified.
  • Conditioning: laboratories condition specimens in the standard atmosphere for textiles (ISO 139: 20 °C and 65 % relative humidity) before measuring. An in-house check without a conditioning room should at least let the sample rest flat and cool before both measurements.

How to do a shrinkage test, step by step

  1. Cut the specimen. Take a piece large enough for your gauge marks with a margin, commonly 50 cm × 50 cm marks on a sample of about 60 cm × 60 cm. Note the roll, lot and side.
  2. Condition it. Let the specimen lie flat without tension (in a conditioning room for a lab test) so the first measurement is not taken on stretched fabric.
  3. Mark it. Mark at least three gauge lengths in the warp or wale direction and three in the weft or course direction, for example 50 cm each, using the template. Number the marks.
  4. Measure before washing. Measure each gauge length and write the values down. Do not assume they are exactly 50.0 cm; measure them.
  5. Wash and dry. Wash with the stated load, detergent, temperature and programme, then dry by the stated method. Repeat for the number of cycles the buyer specifies (often one or three).
  6. Condition and smooth. Let the specimen recover flat without stretching; lay it on a smooth table and remove wrinkles by hand without pulling.
  7. Measure after washing and calculate. Measure the same gauge lengths, calculate the change for each, average the warp and weft values separately and compare them with the buyer's limit.

Fabric shrinkage formula, with worked examples

The fabric shrinkage test formula, as used in ISO 5077 and in most buyer manuals, is:

Dimensional change % = (measurement after washing − measurement before washing) ÷ measurement before washing × 100

The sign tells you the direction. A negative result means the fabric got shorter or narrower (shrinkage). A positive result means it got longer or wider (growth, sometimes called extension). Some reports drop the minus sign and write "shrinkage 4.4 %"; say which convention you use on the report.

Worked example (sample data): a single jersey specimen marked with 50.0 cm gauge lengths.

DirectionBefore (cm)After (cm)CalculationResult
Warp / length (average of 3 marks)50.047.8(47.8 − 50.0) ÷ 50.0 × 100−4.4 % (shrinkage)
Weft / width (average of 3 marks)50.051.0(51.0 − 50.0) ÷ 50.0 × 100+2.0 % (growth)

Knits often behave like this example: they shrink in length and grow slightly in width, because the loops shorten and spread. Wovens more often shrink in both directions, typically more in the warp.

Two more worked figures to check your arithmetic: a 50.0 cm mark that measures 48.5 cm after washing is (48.5 − 50) ÷ 50 × 100 = −3.0 %; a 35.0 cm mark that measures 34.3 cm is −2.0 %. Always average the three marks in each direction before comparing with the limit; one mark can be off because of a crease or a stretched edge.

What shrinkage is acceptable?

The buyer sets it, per fabric and garment type. Requirements are usually written as a range for each direction, for example "−5 % to +3 %" or "±5 %", sometimes tighter for fitted garments or looser for heavy fleece. There is no universal figure, and you should not use a number from another buyer's manual. In our worked example, a buyer limit of ±5 % would pass both directions (−4.4 % and +2.0 %) while a limit of −3 % to +2 % would fail the warp result. These limits are sample data for illustration, not recommended limits.

When a result is close to the limit, test a second specimen from a different roll before deciding: shrinkage varies with the finishing batch, and one specimen is not a lot.

Knit vs woven: what changes?

The method is the same, but knits need two extra cautions. First, they stretch easily, so marking and measuring must be done flat and without tension; a ruler pressed along a jersey sample will stretch it by several millimetres. Second, single jersey in particular can twist after washing, so the side seams of a T-shirt move round the body. That is spirality, measured as an angle or a percentage under ISO 16322, and many knit buyers ask for it alongside dimensional change. Wovens can show skew after washing instead, which is related to the bow and skew measured during fabric inspection under ASTM D3882.

Knits are also the fabrics most affected by relaxation before cutting. Relaxation shrinkage, the change while the fabric rests unrolled, is different from wash shrinkage; our page on fabric relaxation before cutting explains how to time and measure it.

How to adjust patterns for shrinkage

If you know a fabric will shrink and the buyer accepts it within limits, the pattern can be cut larger so the finished garment lands on size. The compensation formula is:

Cut length = finished length ÷ (1 − shrinkage as a decimal)

For a body length of 70 cm in a fabric that shrinks 4.4 % in length: 70 ÷ (1 − 0.044) = 70 ÷ 0.956 = 73.22 cm. Adding 4.4 % to 70 cm (73.08 cm) is a common shortcut, but it under-compensates, because the shrinkage applies to the larger cut piece, not to the finished size.

ShrinkageDivide byFinished 50 cm → cutFinished 70 cm → cutFinished 100 cm → cut
2 %0.9851.02 cm71.43 cm102.04 cm
3 %0.9751.55 cm72.16 cm103.09 cm
4 %0.9652.08 cm72.92 cm104.17 cm
5 %0.9552.63 cm73.68 cm105.26 cm
6 %0.9453.19 cm74.47 cm106.38 cm

Compensate the warp and weft directions separately with their own figures; a knit that shrinks in length and grows in width needs the width reduced, not increased. Pattern compensation only works when shrinkage is consistent across the lot, which is one more reason to test more than one roll.

Shrinkage test report format

Whether the test was done in-house or by a laboratory, a usable shrinkage test report contains:

FieldExample (sample data)
Report no., dateSH-0318, 03 Nov 2026
Buyer, PO, styleExample buyer, PO-4512, NB-TEE-102
Fabric, GSM, lot / rollSingle jersey 180 GSM, lot L-KN-2195, roll N-45012
MethodISO 6330 wash programme as per buyer manual, line dry, measured to ISO 5077
Cycles1
Gauge length50.0 cm, 3 marks per direction
Warp / length change−4.4 % (marks: −4.2, −4.4, −4.6)
Weft / width change+2.0 %
Spirality (knits)As required, e.g. per ISO 16322
Buyer requirement±5 % each direction (sample)
Verdict, tested by, checked byPASS · lab technician · QC head

A printable version of this table is the simplest shrinkage test report template: print this page from your browser (Ctrl+P, or Share → Print on Android) and fill in the right-hand column for each test.

Record shrinkage per roll and lot in the app

Fabric Inspection Software records wash shrinkage in warp and weft on the roll record, next to the 4-point result, GSM, shade and width checks, and prints it on the buyer report. When the shrinkage comes from a laboratory, the fabric test register keeps the full report by lot and PO: dimensional stability to washing is one of its standard methods, judged line by line against each buyer's range, with the lab's PDF attached and an alert before the report expires. Relaxation before cutting is tracked separately on the relaxation board. See every capability on the features page, plans from ₹4,999 a month on the pricing page, and how shrinkage fits into roll inspection in our guide to inspecting knitted fabric with the 4-point system.

Questions people ask

How do you calculate fabric shrinkage percentage?

Subtract the measurement before washing from the measurement after washing, divide by the measurement before washing and multiply by 100. A 50.0 cm mark that measures 47.8 cm after washing gives (47.8 − 50.0) ÷ 50.0 × 100 = −4.4 %. A negative result is shrinkage, a positive result is growth.

What is the standard method for a shrinkage test?

Many buyers name ISO 3759 for marking and measuring, ISO 6330 for the washing and drying procedure and ISO 5077 for the calculation; US buyers often name AATCC 135 instead. The buyer's manual gives the exact programme, temperature, drying method and number of cycles, so always test to the manual.

What is acceptable shrinkage for cotton knit fabric?

Whatever the buyer's manual allows for that fabric and garment. Requirements are usually written per direction, for example a range such as −5 % to +3 %, and they differ between buyers. Do not borrow a limit from another buyer; Fabric Inspection Software stores each buyer's own range and judges results against it.

Is shrinkage measured before or after relaxation?

Wash shrinkage is measured on a conditioned, relaxed specimen before and after washing, so the specimen should rest flat without tension before the first measurement. Relaxation shrinkage before cutting is a separate figure: the change in width and length while rolls rest unrolled. Record both; they answer different questions.

How many washes are used in a shrinkage test?

The buyer's method decides. Many programmes use one wash and dry cycle, and some ask for three or more to see whether the fabric keeps shrinking. Write the number of cycles on the report, because a result after one cycle cannot be compared with a limit written for three.

What is the difference between shrinkage and growth?

Shrinkage is a decrease in length or width after washing and is reported as a negative percentage; growth, or extension, is an increase and is reported as positive. Knits often shrink in length and grow slightly in width in the same test, so warp and weft are always reported separately.

How do you adjust a pattern for fabric shrinkage?

Divide the finished measurement by one minus the shrinkage as a decimal. A 70 cm body length in fabric that shrinks 4.4 % becomes 70 ÷ 0.956 = 73.22 cm on the pattern. Compensate warp and weft separately, and only when shrinkage is consistent across the lot.

Related guides

Inspect the first roll the same day

We load your defect master, buyer limits and report layout, then train your inspectors on the floor in Tirupur, Surat or Ludhiana, or over a video call. 14-day pilot, no card. Plans start at ₹4,999 a month with unlimited rolls, and every result follows the ASTM D5430 4-point rules and your buyer's own limit.